VLU-300, VLU-500 and VLU-800
Protector Fleeces
APP Protector
Fleeces guard the surface of the roof from damage. The greater the
stress to which the installation is subjected, the stronger the
protection fleece will need to be. The protection layer is laid over a root-resistant seal or root barrier.
The fleeces inhibit root growth after installation. The technical
data of the APP Protective fleeces comply with the requirements of
DIN 18195. |
|
VLS-500/800 Water-Retentive
Fleece
The VLS Water-retentive fleece, which is made from
very thin fibres, protects the roof Fleece and retains water and
nutrients for the plants. It is installed above the root-proof
barrier. The fleece can absorb seven times its own weight of water.
A certificate for this performance is available.
|
|
|
Protector
|
Storage and
Protector
|
|
VLU-300
|
VLU-500
|
VLU-800
|
VLS-500
|
VLS-800
|
|
Protector
layer for extensive roof garden projects
|
Protector
layer for intensive roof garden projects RGP
|
High-grade
(Hi-G) Protector layer for intensive RGP
|
Protector
and reservoir for extensive or intensive RGP
|
Protector
and reservoir for extensive or intensive
RGP Hi-G
|
|
300
|
500
|
800
|
480
|
800
|
|
3,0
|
4,5
|
5,5
|
3,3
|
4,8
|
|
20
|
29
|
35
|
0,7
|
0,85
|
|
28
|
49
|
50
|
0,85
|
1,50
|
|
60/60
|
70/65
|
50/80
|
90/80
|
120/80
|
|
3600
|
7000
|
9684
|
2700
|
3700
|
|
3300
|
6500
|
9060
|
|
|
|
4
|
5
|
5
|
4
|
5
|
|
0,08
|
0,11
|
-
|
0,06
|
0,07
|
|
2,4*10-3
|
2,3*10-3
|
3,1*10-3
|
5,0
|
8,0
|
|
Polypropylene
|
|
0,9
|
0,9
|
0,9
|
-
|
-
|
|
±165
|
±165
|
±165
|
±165
|
±165
|
|
Mechanically hardened, thermally treated
|
Mechanically hardened
|
|
2,5
|
2,5
|
2,5
|
2,2
|
2,2
|
|
50
|
50
|
50
|
50
|
25
|
|
125
|
125
|
125
|
110
|
55
|
|
40
|
65
|
100
|
55
|
48
|
|
45
|
50
|
50
|
50
|
48
|
|
White
|
White
|
White
|
Melange-Grey
|
Melange-Grey
|
|
|
Different weights per unit area and roll
dimensions may be produced to the customer's requirements. The
products should not be exposed to direct sunlight for longer than
four weeks, as they are not UV-stabilised. All the values presented
in this table are averages from standard tests. In practice, slight
fluctuations occur in actual production. Consistency in production
according to DIN ISO 9001 is assured. We reserve the right to change
amend specifications.
|
|